Improving the Abrasion Resistance of "Green" Tyre Compounds
Later, the masterbatches were sheeted out on a warm tworoll mill with minimal passes. In the second stage, the masterbatches were remilled in the same mixer for 3 minutes with a rotor speed of 80 rpm and starting temperature of 80°C. Then the masterbatches were sheeted out on warm tworoll mill .